Ilmenite

Fe²⁺TiO₃ · oxide

Ilmenite is the second titanium mineral at Orión — present in the bulk channel samples, but the smaller of the two in an assemblage Osmond describes as rutile-dominant.

Yields

→ titanium

Data status

Assayed / quantified

Class

oxide

Why it matters

As general mineralogy, not an Osmond figure, ilmenite carries markedly less titanium dioxide than rutile does — about 35–65% TiO₂ against natural rutile's roughly 95% — so which of the two minerals dominates an assemblage matters more than the combined titanium content on its own.

At Orión the balance falls the way it does. On a mass-balance basis dated 19 February 2026, bulk channel samples returned 4.82–6.19% ilmenite, the smaller titanium mineral in a rutile-dominant assemblage; Osmond describes rutile as outweighing ilmenite by roughly two to one or more. Those are grades for the channel samples. The same 19 February 2026 samples carry total heavy minerals of 29.4–32.8%, with up to roughly 40% estimated in the AV-01bis interval.

One qualification travels with the number. Like every mineral percentage in the reported assemblage, the ilmenite figure is a mass-balance estimate calculated from oxide assays rather than a directly measured mineral content.

Quantified in the bulk channel samples on a mass-balance basis only; no concentrate grade, no recovery, and no deposit-wide grade.

Used for

  1. 01TiO₂ pigment — the white in paint, plastics and paper.
  2. 02Sulfate-route feedstock — the process that takes lower-grade titanium minerals directly.
  3. 03Synthetic rutile — upgraded ilmenite as a higher-titanium feed.

Latest on Ilmenite

A wide upland of dry grass and pale limestone, ridges receding into haze under a bright overcast sky.Mining & ProductionOrión Project Overview7 min readA pale rock face crossed by dark vertical bands, with a geological hammer and hand lens resting on a ledge below them.Mining & ProductionReading the Orión seams: what the heavy-mineral layers tell us6 min readA mound of very fine white powder on a dark textured surface, lit from one side so its ridges and a loose dusting of grains catch the light.Geography & Supply ChainsEurope owns the middle of titanium — and neither end.5 min readA machined metal impeller with curved blades cut integrally from a single disc, lit from one side on a dark tray.Applications & IndustriesWhy aerospace still can't design titanium out4 min readA broad stroke of thick white paint drawn across weathered grey-brown timber, hiding the grain beneath it completely.Applications & IndustriesThe white in everything: ilmenite and TiO₂ pigment4 min readA wide beach at low tide, dark streaks of heavy sand fanning in braided lines across pale flats toward a grey sea.Mining & ProductionWhat a lithified placer actually is4 min readA large inclined rotary kiln in a dark industrial hall, its heat-tinted steel shell running away to a glowing discharge end.Mining & ProductionRutile vs ilmenite: why the split matters4 min readA large rotating mill drum discharging coarse crushed rock through a screen onto a conveyor, dust hanging in the air around the frame.Mining & ProductionBreaking rock without breaking the grains6 min readDark grains standing in spiky clusters from a tray of pale sand toward a magnet suspended above it, the sand beneath visibly paler.Mining & ProductionHow two properties sort four minerals6 min readA circular microscope field filled with tightly packed mineral grains in cross-section, pale, dark and brown, each separated by thin boundaries.Innovation & TechnologyThe model that decides which mineral you found6 min readFour large parallel process lines on steel supports, each in different coloured lagging, with control valves and sensors set into them at intervals.Innovation & TechnologyWhat a four-product plant asks of its controls6 min readEight bare cylindrical battery cells standing upright in a loose double row on a scuffed bench, one lying on its side in front.Innovation & TechnologyWhat lithium titanate trades away6 min readFour shallow trays in a row on a bench, each holding a different sand — dark grey, reddish-brown, pale honey and dull yellow-brown.Innovation & TechnologyReconciling a mine that makes four products6 min readA plain grey detector housing mounted on an aluminium tripod in dry sparse grass, a cable running to a small closed case beside one leg.Innovation & TechnologyWhat a thorium channel can and cannot see6 min readAn irregular chunk of bright grey porous metal riddled with open cavities, its broken faces showing the pores running through the mass.Innovation & TechnologyWhy the Kroll process is still standing6 min readA very large reel of bright white paper standing on end, its wound edge a dense pale spiral, with two more reels behind it.Innovation & TechnologyThe uses you can never recycle6 min readA cut face through beach sand banded with many thin dark layers, some continuous and some lensing out, truncating against each other partway up.Geography & Supply ChainsA strandline records which way the sea was going5 min readA large plain white panel lying flat and filling the frame, one small dull grey machined metal part resting near a corner, bench showing along one edge.Geography & Supply ChainsMost titanium ends up as white pigment, not as metal5 min readLow view of a dune crest, a veil of pale sand streaming off it in the wind, ribbons of mixed dark grains lying on the slope below.Mining & ProductionWaves and wind did the first round of mineral sorting5 min readA tall clear glass cylinder of water on a bare grey bench, pale sand settled deep inside it above a thin, sharp layer of near-black grains.Mining & ProductionWhy mineral-sands operations usually concentrate before they separate5 min readThree mineral grains hanging on fine threads against a dark background, a black grain pulled well aside, a brown one slightly, and a pale one hanging straight.Mining & ProductionMagnetic separation matches field strength to the mineral5 min readDrawing of three smooth rolls in a descending cascade, dark grains flung off each in a wide arc while pale grains cling and drop to the next.Mining & ProductionHow a charged roll splits conductors from non-conductors5 min readBlack-and-white micrograph-style image of a single rounded grain in grey relief, a cracked crust clinging to part of its surface and flaking away at one edge.Mining & ProductionWhen cleaning the grains improves separation6 min readTwo single crystals resting well apart on dark slate under even light, a stubby honey-coloured prism on the left and a slender deep red-brown needle on the right.Geography & Supply ChainsWhere the world's zircon and rutile come from5 min readPainting of a shallow sandy seabed in cool blue-green light, faint dark streaks in the rippled sand nearby, fading into murky unlit water a short way off.Geography & Supply ChainsEurope's heavy-mineral sands, by the record5 min read